 Flux cored aluminum electrode

Specification: 1.6/2.0/2.4mm thick, each 50 cm long

Low-temperature aluminum flux-cored welding wire can weld almost all white metals, including aluminum, aluminum alloy, aluminum-magnesium alloy and dissimilar welding between the above metals, even for white metals that have been severely corroded or polluted by oil, and even aluminum that is considered irreparable All alloys can be repaired. Suitable for all-round welding by primary welding operators, only a small heating device is needed, the weld strength after welding is generally higher than the strength of the base metal itself, and it is enough to know the gas welding operation.
Instructions for use of low temperature aluminum welding wire

Step1: through physical cleaning, polish the surface.



Step 2: Heat the surface of the base metal at the welding place until the temperature reaches the working temperature of the welding wire 380℃-400℃, so that the welding wire can be melted by the heat conduction of the base metal to form a weld. Do not use flame to burn the welding wire, and only when the mother When the surface temperature of the material is sufficient, the welding wire can flow and penetrate into the metal capillary well.


Three steps:


When repairing thinner aluminum, just heat the aluminum base material to a suitable working temperature, and then use the welding wire to friction and fuse to form a weld. Only use a metal brush to melt the welding wire to fill the weld to form a weld.


Four steps:


Small parts are welded with propane gas, and large parts are heated and welded with industrial gas or induction heating device. After welding, they will naturally slow down.


Precautions:


The thicker the piece, the more troublesome it will be to heat up, so it is very important to use a reasonable heat source, as long as the surface temperature of the base material reaches the level of the welding wire.


Working temperature, welding can be carried out. When using oxyacetylene welding, use neutral flame welding, but do not directly use fire welding wire


Applicable heat source: It can be used for many kinds of heat sources, such as propane, oxyacetylene, etc.


Storage: Store in a ventilated and dry place for long-term storage
Pay attention to details

1. The surface of the base material must be cleaned. Clean and weld
2. The temperature of the base material must reach 400°C, including the temperature of the base material during the welding process, and the temperature can be high or low.
3. Taboo use flame to burn the welding wire deliberately. After the base metal temperature reaches 400℃, the welding wire will naturally melt by the heat conduction of the base metal.

 Flux cored aluminum electrode

Specification: 1.6/2.0/2.4mm thick, each 50 cm long

Low-temperature aluminum flux-cored welding wire can weld almost all white metals, including aluminum, aluminum alloy, aluminum-magnesium alloy and dissimilar welding between the above metals, even for white metals that have been severely corroded or polluted by oil, and even aluminum that is considered irreparable All alloys can be repaired. Suitable for all-round welding by primary welding operators, only a small heating device is needed, the weld strength after welding is generally higher than the strength of the base metal itself, and it is enough to know the gas welding operation.
Instructions for use of low temperature aluminum welding wire

Step1: through physical cleaning, polish the surface.



Step 2: Heat the surface of the base metal at the welding place until the temperature reaches the working temperature of the welding wire 380℃-400℃, so that the welding wire can be melted by the heat conduction of the base metal to form a weld. Do not use flame to burn the welding wire, and only when the mother When the surface temperature of the material is sufficient, the welding wire can flow and penetrate into the metal capillary well.


Three steps:


When repairing thinner aluminum, just heat the aluminum base material to a suitable working temperature, and then use the welding wire to friction and fuse to form a weld. Only use a metal brush to melt the welding wire to fill the weld to form a weld.


Four steps:


Small parts are welded with propane gas, and large parts are heated and welded with industrial gas or induction heating device. After welding, they will naturally slow down.


Precautions:


The thicker the piece, the more troublesome it will be to heat up, so it is very important to use a reasonable heat source, as long as the surface temperature of the base material reaches the level of the welding wire.


Working temperature, welding can be carried out. When using oxyacetylene welding, use neutral flame welding, but do not directly use fire welding wire


Applicable heat source: It can be used for many kinds of heat sources, such as propane, oxyacetylene, etc.


Storage: Store in a ventilated and dry place for long-term storage
Pay attention to details

1. The surface of the base material must be cleaned. Clean and weld
2. The temperature of the base material must reach 400°C, including the temperature of the base material during the welding process, and the temperature can be high or low.
3. Taboo use flame to burn the welding wire deliberately. After the base metal temperature reaches 400℃, the welding wire will naturally melt by the heat conduction of the base metal.

Shipping And Delivery

RazzX

Free Shipping

We are glad to bring our customers great value and service. That’s why we provide free shipping from our warehouses in Asia by E-Packet or EMS and in USA by USPS.

Shipping to Over 200 Countries

We are proud to offer international shipping services. However, there are some locations we are unable to ship to. If you happen to be from one of those countries we will contact you.

Lost/Missing Packages

RazzX are not liable if the incorrect address is placed during the checkout process. Please make sure that your billing and shipping address is correct before processing your order. If we have made an error we will fully take responsibility of the original order that was made for you at no charge.

Customs

We are not responsible for any custom fees once the items have shipped. By purchasing our products, you consent that one or more packages may be shipped to you and may get custom fees when they arrive in your country.

Shipping Time

Shipping time varies by location. These are our estimates:

Location *Estimated Shipping Time
United States 8-14 Business days
Canada, Europe 8-15 Business days
Australia, New Zealand 8-15 Business days
Central & South America 10-20 Business days
Asia 8-15 Business days
Africa 15-30 Business days

Tracking Information

You will receive an email with a tracking number once your order is shipped but sometimes due to free shipping tracking is not available.

My Tracking Says “No Information Available At The Moment”

For some shipping companies, it takes 2-5 business days for the tracking information to update on the system. If your order was placed more than 5 business days ago and there is still no information on your tracking number, please contact us.

Will My Items Be Sent In One Package?

For logistical reasons, items in the same purchase will sometimes be sent in separate packages, even if you’ve specified combined shipping.

If you have any other questions, please contact us and we will do our best to help you out.

View full details
1 of 5